Flow disruption - International Powder Systems 2022

Go to content

Flow disruption

Troubleshooting

Cause

Correction

Particle size distribution of the powder is too coarse.

Contact powder suppliers.

Contamination.

Contamination by foreign powder can be avoided by careful cleaning of the plant. In addition, different powders should not be mixed.

Too high or too low film thicknesses.

Adjust powder output.

Too wet or too hot workpieces.

Check drying and temperature of the workpieces.

Powder deposits accumulate on nozzles.

Maintenance!

Drop formation occurs when the powder flow is too strong.

Verification of the voltage and the distance to the workpiece, or the addition of thixotroping agents can help.